Use of Adhesion Promoters

 

Application

Apply a thin coat to the solvent cleaned surface with clean gauze and allow to dry for approximately 30 minutes at standard temperature (77°F at 50% RH).  After drying time, wipe off excess with a clean gauze pad and start the sealant procedure. If surface becomes contaminated or sealing is not accomplished with 4 hours after application of the adhesion promoter, repeat priming procedure.

 

Product
Features
Chemistry
Bonds
PR-142* Non-crazing for Acrylic and Polycarbonate Silane Glass
Polycarbonate
Acrylic
PR-148 Cleaner and coupling agent Titanate Fuel soaked sealant
Aged paints and primers
Stainless steel
Titanium
PR-182 VOC compliant
Water based
worker/environmentally friendly
Silane
PR-187 Coupling agent for polythioether
to polysulfide applications
Epoxy All surfaces

*Note that PR-142 is used for some polythioether applications

 

All recommendations, statements, and technical data contained herein are based on tests we believe to be reliable and correct, but accuracy and completeness of said tests are not guaranteed and are not to be construed as a warranty, either expressed or implied. User shall rely on his own information and tests to determine suitability of the product for the intended use and assumes all risks and liability resulting from his use of the product.

Bergdahl Associates, Inc. 775-323-7542